♦ Igama locingo lwe-Weliding: ErNiCr-3, Inconel 82 TIG/MIG Wire
♦ MOQ:15kg
♦ Ifom: MIG(15kgs/spool), TIG(5kgs/box)
♦ Ubungakanani:Ububanzi 0.01mm-8.0mm
♦ Ubungakanani obuqhelekileyo:0.8MM / 1.0MM / 1.2MM / 1.6MM / 2.4MM / 3.2MM / 3.8MM / 4.0MM / 5.0MM
♦ Imigangatho:Iyahambelana neSiqinisekiso AWS A5.14 ASME SFA A5.14
I-ErNiCr-3 yi-nickel-base alloy wire ye-72Ni20C ye-nickel-chromium molybdenum series.
Intsimbi yokugquma ineempawu ezilungileyo zoomatshini, ukuxhathisa okulungileyo kwe-corrosion, ukuxhathisa kwe-oxidation, amandla aphezulu ahambayo, i-arc ezinzileyo, imilo entle, ukumanzi kakuhle kwentsimbi etyhidiweyo, kunye nokusebenza kakuhle kwenkqubo ye-welding.
C | Cr | Ni | Si | Mn | P | S | Nb+Ta | Fe |
≤0.1 | 18.0-22.0 | ≥67 | ≤0.5 | 2.5-3.5 | ≤0.03 | ≤0.015 | 2.0-3.0 | ≤3.0 |
Ububanzi | Inkqubo | IVolt | Amps | Irhasi yokuKhusela | |
In | mm | ||||
0.035 | 0.9 | GMAW | 26-29 | 150-190 | UTshintsho lokutshiza100% Argon |
0.045 | 1.2 | 28-32 | 180-220 | ||
1/16 | 1.6 | 29-33 | 200-250 | ||
1/16 | 1.6 | GTAW | 14-18 | 90-130 | 100% Argon |
3/32 | 2.4 | 15-20 | 120-175 | ||
1/8 | 3.2 | 15-20 | 150-220 |
Imeko | Ukuqina kokuqina kweMPa (ksi) | Isivuno Amandla eMPa (ksi) | Elongation% |
AWS reauirement | 550(80) | Ayichazwanga ngqo | Ayichazwanga ngqo |
Iziphumo eziqhelekileyo njengoko zidityanisiwe | 460(67) | 260(38) | 28 |
S Ni6082 , AWS A5.14 ERNiCr-3 , EN ISO18274
Isetyenziselwa ukuwelda i-Inconel 600601690 ingxubevange, i-Incoy 800800HT330 ingxubevange, ingasetyenziselwa ukusetyenzwa komphezulu wentsimbi ye-ErNiCr-3 yocingo lwentsimbi ye-weld inamandla aphezulu kunye nokuxhathisa okuhle kokubola, inokumelana ne-oxidation elungileyo kwiqondo lobushushu obuphezulu kunye namandla aphezulu okuqhekeka.
Indawo yesicelo ye-ERNiCr-3:
I-ERNiCr-3 i-welding wire isetyenziswa ngokubanzi kwizinto ezingafaniyo, i-welding material, ezifana ne-Inconel series alloy, i-Inconel series alloy welding, okanye i-Incoloy 330 alloy kunye nocingo, i-Monei series alloy kunye nentsimbi engatyiwayo kunye ne-carbon steel welding, ingasetyenziselwa ukuwelda. insimbi engenasici kunye ne-nickel-based alloy okanye i-carbon steel.